Molybdenum dioxide is used as an electrode and catalyst material, and as a component in lithium battery and supercapacitor research. It decomposes rather than melting cleanly, so target density and bonding decide whether it survives a run.
Specification
| Composition | MoO2 |
|---|---|
| Purity | 99.9% |
| Density | 6.47 g/cm³ |
| Melting point | ≈1100 (decomposes) °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- MoO2 decomposes before melting — thermal management is critical.
- Density above 95% is typical; porosity shows as particles.
- For battery work, the film phase and nanostructure matter more than purity.
End applications
- Electrode and catalyst films
- Lithium battery and supercapacitor research
- Gas sensors
- Optical absorber layers
Frequently asked
Why does my MoO2 target crack?
Thermal stress from poor bonding or a fast ramp. The material decomposes rather than melting, so the target cannot redistribute heat by melting.
Do you supply MoO3 as well?
MoO3 is a separate product used as a hole-injection layer; both are available.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.





Reviews
There are no reviews yet.