Hematite targets deposit the alpha-phase iron oxide used in photoelectrochemical water splitting, gas sensing and as a magnetic underlayer. The phase — hematite versus magnetite — determines whether the film is an insulator or a conductor.
Specification
| Composition | Fe2O3 (hematite) |
|---|---|
| Purity | 99.9–99.99% |
| Density | 5.24 g/cm³ |
| Melting point | 1565 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- Phase purity matters: Fe2O3 and Fe3O4 give different electrical and magnetic behaviour.
- Oxygen stoichiometry shifts the film between phases; the target sets the starting point.
- For photoanodes, film thickness and doping dominate performance.
End applications
- Photoelectrochemical water splitting
- Gas sensors
- Magnetic and spintronic layers
- Pigment and decorative films
Frequently asked
What is the difference between Fe2O3 and Fe3O4 targets?
Hematite (Fe2O3) is an insulator, magnetite (Fe3O4) is a conductor with different magnetic behaviour. They are separate products.
Is the phase stated on the certificate?
Yes — phase and stoichiometry are reported for iron oxide targets.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.