Specification

Composition Cr2O3
Purity 99.9%
Density 5.22 g/cm³
Melting point 2435 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • Stoichiometry affects colour and hardness — CrOx with x below 1.5 looks different.
  • Targets are insulators; RF sputtering is required.
  • For decorative black coatings, the process gas composition is as important as the target.

End applications

  • Decorative black and grey coatings
  • Wear-resistant layers
  • Corrosion barriers
  • Optical absorber layers

Frequently asked

Can Cr2O3 be sputtered reactively from chromium metal?

Yes, and that is common in production. A ceramic Cr2O3 target is used where a fixed stoichiometry is preferred.

Why does the film colour vary?

Stoichiometry and thickness. CrOx colour depends strongly on the oxygen content of the film.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Chromium Oxide (Cr₂O₃) Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us