Zirconium Oxide (ZrO₂) Sputtering Target

3N–4N (99.9–99.99%)DiscSintering

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Zirconium dioxide is used as a tough, high-index layer that survives thermal cycling better than TiO2, and as a thermal barrier in coated tooling. Its high melting point makes the target hard to densify, so density is the value to check.

Specification

Composition ZrO2
Purity 99.9–99.99%
Density 5.68 g/cm³
Melting point 2715 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • High melting point makes full densification difficult — ask for the density figure.
  • ZrO2 can exist in monoclinic, tetragonal or cubic phase; the phase affects film stress.
  • For tool coatings, yttria-stabilised zirconia is often preferred.

End applications

  • Laser and optical coatings
  • Thermal barrier layers
  • Wear-resistant tool coatings
  • Solid oxide fuel cell research

Frequently asked

Why is ZrO2 density often lower than other oxides?

The high melting point limits sintering. Dense targets need hot pressing or sintering aids, and the density should be stated.

Do you supply yttria-stabilised zirconia?

Yes — YSZ targets are quoted to the yttria content you specify.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews