Zinc oxide targets serve two very different purposes: a transparent conductive oxide when doped with aluminium (AZO), and a piezoelectric or buffer layer when undoped. The undoped target is also used reactively, where the oxygen flow decides the film properties more than the target does.
Specification
| Composition | ZnO |
|---|---|
| Purity | 99.9–99.99% |
| Density | 5.61 g/cm³ |
| Melting point | 1975 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- For AZO, specify the Al2O3 content (1–2 wt%) — this is a different target, not a process tweak.
- ZnO is sensitive to oxygen partial pressure; small changes shift carrier concentration.
- Targets are hot-pressed; density affects both arcing and film uniformity.
End applications
- AZO transparent conductors
- Piezoelectric ZnO films
- Buffer layers in solar cells
- Gas sensors and varistors
Frequently asked
Can I make AZO from a pure ZnO target?
Not reliably. Aluminium doping is set in the target; reactive co-sputtering is possible but hard to control. We supply Al-doped targets to your wt%.
What density do you supply?
Typically 97–99% of theoretical, stated on the certificate.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.





Reviews
There are no reviews yet.