Silver (Ag) Foil 4N

4N (99.99%)Foilrolling

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Silver foil in 4N purity from 0.02 mm, for contacts, EMI gaskets and evaporation sources. Silver has the lowest resistivity of any metal, so a thin foil carries more current than a copper one of the same thickness.

Specification

Metal Silver (Ag)
Purity 4N (99.99%)
Form Foil
Dimensions Thickness 0.02–0.5 mm; width 10–100 mm; cut pieces
Density 10.49 g/cm³
Melting point 962 °C
Packing Vacuum-sealed, argon flushed; spool or flat pack in a foam-lined case
MOQ 100 g (samples from 10 g)
Lead time 10–20 working days

Tolerances and handling

  • Silver foil work-hardens quickly; specify whether you need annealed or hard temper.
  • Thin foil below 0.05 mm is fragile — flat packing, not coiling.
  • Sulphur in packaging materials can tarnish the surface; use sulphur-free interleaving.

End applications

  • Electrical contacts and busbar shims
  • EMI shielding gaskets
  • Evaporation source for low-E and optical coatings
  • Brazing foil for ceramic-to-metal seals

Frequently asked

Can silver foil be soldered?

Yes, but silver dissolves in tin-based solders. Use a silver-bearing solder or a nickel barrier if the joint must survive multiple reflows.

What widths are available?

10–100 mm standard; wider on request up to 200 mm.

Related reading: all wire, foil and solder products · high-purity evaporation materials

Related resources

Reviews

There are no reviews yet.

Be the first to review “Silver (Ag) Foil 4N”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us