High-Purity Aluminium (Al) Wire 5N

5N (99.999%)Wiredrawing

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

High-purity aluminium wire at 5N (99.999%), from 0.5 mm to 3.0 mm, supplied on spools. This is the grade used for semiconductor metallisation and for evaporation feed where the film is an electrical layer rather than a decorative one.

Specification

Metal Aluminium (Al)
Purity 5N (99.999%)
Form Wire
Dimensions Ø 0.5–3.0 mm; spools of 100 g–1 kg
Density 2.70 g/cm³
Melting point 660 °C
Packing Vacuum-sealed, argon flushed; spool or flat pack in a foam-lined case
MOQ By agreement — quoted per order
Lead time 10–20 working days

Tolerances and handling

  • Aluminium wire is soft and galls; the spool tension matters as much as the diameter.
  • For bonding wire, the surface finish and oxide thickness are specified — ask for the drawing.
  • Store sealed: aluminium oxide grows slowly but changes the first-melt behaviour.

End applications

  • Semiconductor metallisation and bonding
  • Evaporation feed for e-beam sources
  • High-purity contacts
  • Analytical standards

Frequently asked

Why 5N rather than 4N?

For semiconductor films the trace metal level affects resistivity and junction behaviour; 4N is adequate for decorative and packaging work.

Do you supply aluminium bonding wire?

We supply the material; bonding wire with controlled elongation is quoted against your machine specification.

Related reading: all wire, foil and solder products · high-purity evaporation materials

Related resources

Reviews

There are no reviews yet.

Be the first to review “High-Purity Aluminium (Al) Wire 5N”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us