Niobium targets are used for superconducting films (Nb, NbN), for barrier layers and — increasingly — as a component of high-entropy and Nb-based oxide coatings. In superconducting work the residual resistance ratio is dominated by the target purity and by oxygen.
Specification
| Material | Niobium (Nb) |
|---|---|
| Purity | 3N5–4N (99.95–99.99%) |
| Density | 8.57 g/cm³ |
| Melting point | 2477 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing |
| Grain / texture | Fine grain; stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Oxygen and nitrogen raise the residual resistance; ask for the gas figures for superconducting films.
- Niobium is soft and galls; machined surfaces must be handled carefully.
- For NbN, reactive sputtering with a controlled nitrogen flow gives better stoichiometry than a ceramic target.
End applications
- Superconducting films and Josephson junctions
- Diffusion barriers and interconnects
- Corrosion-resistant coatings
- Optical and decorative films
Frequently asked
Do you supply ultra-high-purity niobium?
We supply 3N5 as standard and can quote 4N with a GDMS certificate for superconducting work.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.