Silver wire in 4N purity, drawn from 0.025 mm (1 mil) to 6.0 mm. The highest electrical and thermal conductivity of any metal, supplied annealed on spools for contacts, brazing and evaporation feed.
Specification
| Metal | Silver (Ag) |
|---|---|
| Purity | 4N (99.99%) |
| Form | Wire |
| Dimensions | Ø 0.025–6.0 mm; coils or straight lengths |
| Density | 10.49 g/cm³ |
| Melting point | 962 °C |
| Packing | Vacuum-sealed, argon flushed; spool or flat pack in a foam-lined case |
| MOQ | 100 g (samples from 10 g) |
| Lead time | 10–20 working days |
Tolerances and handling
- Silver tarnishes in sulphur-bearing air; store sealed and use within the stated shelf life.
- Fine wire is annealed and soft — avoid sharp bends when routing.
- For brazing alloys, silver wire is often supplied as part of a preform rather than as straight wire.
End applications
- Electrical contacts and fuse elements
- Brazing and joining
- Evaporation feed wire
- Conductive gaskets and shielding
Frequently asked
Does silver wire tarnish in storage?
Yes, in air containing sulphur. Vacuum-sealed packing with short shelf life is standard; tarnish can be removed chemically but affects bonding.
Is 5N silver available?
4N is standard; 5N can be quoted for specific lots with a GDMS certificate.
Related reading: all wire, foil and solder products · high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.