Hafnium dioxide is the UV-capable high-index material: it transmits further into the ultraviolet than Ta2O5 or TiO2, and it has the highest laser damage threshold of the common oxides. It is also a high-k dielectric in semiconductor work.

Specification

Composition HfO2
Purity 99.9–99.99%
Density 9.68 g/cm³
Melting point 2758 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • The material of choice for UV and high-power laser coatings.
  • Very high melting point — density and bonding decide whether the target survives.
  • Hafnium is expensive; utilisation and reclaim matter.

End applications

  • UV and excimer laser optics
  • High-power laser coatings
  • High-k dielectrics
  • Anti-reflection coatings for deep UV

Frequently asked

Why HfO2 for UV coatings?

It transmits where Ta2O5 and TiO2 absorb, and its laser damage threshold is higher. The trade-off is cost and deposition rate.

Is nuclear-grade hafnium-free zirconium relevant here?

That concerns zirconium metal, not HfO2. For HfO2, the specification is purity and phase.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Hafnium Oxide (HfO₂) Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us