Tantalum Sputtering Target 3N5-4N5

3N5–4N5 (99.95–99.995%)DiscMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Tantalum is the barrier metal of choice where copper must not migrate and where a film has to survive high temperature. It is dense, hard to machine and expensive, so target utilisation and reclaim weigh on the cost per wafer more than the sputter rate does.

Specification

Material Tantalum (Ta)
Purity 3N5 (99.95%) – 4N5 (99.995%)
Density 16.65 g/cm³
Melting point 3017 °C
Form Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing · rotatables on request
Grain / texture Fine grain, controlled texture — stated on request
Bonding Indium or elastomer to Cu / Al backing, bond coverage checked
Packing Vacuum-sealed, foam-lined case with flatness record
MOQ 1 pc
Lead time 15–25 working days

Sputtering notes

  • Tantalum targets are usually made by vacuum melting or powder metallurgy; the route determines grain size and oxygen content.
  • High oxygen gives a resistive beta-phase film — specify gas content for barrier work.
  • Bonding is essential for large planar targets; unbonded tantalum cracks under thermal cycling.

End applications

  • Diffusion barriers for copper interconnects
  • Capacitor and gate electrodes
  • Wear and corrosion-resistant coatings
  • Implant and medical device coatings

Frequently asked

Alpha or beta phase?

The phase of the deposited film depends on the target and the process; for barrier work you want the low-resistivity alpha phase, which needs low oxygen in the target.

Do you supply tantalum rotatables?

Yes — rotary targets for high-volume lines, quoted against the tool geometry.

Related reading: target specification guide · all metal sputtering targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Tantalum Sputtering Target 3N5-4N5”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us