Tin targets are used for solderable layers, for transparent oxide research and as an alloying component in Sn-based films. Like zinc and indium, tin melts low — at 232 °C — so the process window sits between “not hot enough to sputter well” and “hot enough to melt the target”.
Specification
| Material | Tin (Sn) |
|---|---|
| Purity | 4N–5N (99.99–99.999%) |
| Density | 7.28 g/cm³ |
| Melting point | 232 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing |
| Grain / texture | Fine grain; stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Low melting point — bonding and power control are both essential.
- Tin grows whiskers under stress; films intended for electronics need a cap layer.
- For solderable finishes, a SnAg or SnCu alloy target often outperforms pure tin.
End applications
- Solderable surface finishes
- Tin oxide and transparent conductor research
- Corrosion-resistant coatings
- Alloy films for electronic assembly
Frequently asked
Why use a SnAg target instead of pure tin?
Whisker growth and melting behaviour. Alloyed films are more stable under thermal cycling, which matters for connectors and PCB finishes.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.