Nickel targets are usually specified for what the film enables — a diffusion barrier, a solderable surface, a magnetic layer in a stack — rather than for the nickel itself. Sulphur and iron are the impurities that matter, and both are reported on the certificate.
Specification
| Material | Nickel (Ni) |
|---|---|
| Purity | 3N5 (99.95%) – 4N5 (99.995%) |
| Density | 8.90 g/cm³ |
| Melting point | 1455 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing · rotatables on request |
| Grain / texture | Fine grain, controlled texture — stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Sulphur segregates to the target surface and causes film haze; specify its level explicitly.
- Nickel is ferromagnetic — a magnetically compensated magnetron gives a more uniform erosion profile.
- Fine grain reduces the nodule formation that plagues soft magnetic targets.
End applications
- Diffusion barriers and adhesion layers
- Seed layers for soldering and plating
- Magnetic film stacks with Fe and Co
- Decorative and corrosion-resistant coatings
Frequently asked
Why is sulphur important in a nickel target?
It segregates and causes haziness and adhesion loss in the deposited film. For 4N5 we report it in the impurity table.
Can I sputter Ni with a standard magnetron?
Yes, but the magnetic field will be distorted; a compensated cathode gives better uniformity.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.