Silicon monoxide is used mainly as an evaporation material for optical and protective coatings, and as a sputtering target where a sub-stoichiometric silicon oxide film is wanted. Its low density and reactivity make dense targets difficult to produce.
Specification
| Composition | SiO |
|---|---|
| Purity | 99.9% |
| Density | 2.13 g/cm³ |
| Melting point | 1702 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- SiO is reactive and disproportionates at temperature — handle and store sealed.
- For optical coatings, the film index depends on the oxygen content.
- Density is lower than SiO2; targets are fragile.
End applications
- Optical coatings with tuned index
- Protective and release layers
- Evaporation source for SiO films
- Barrier layers in packaging
Frequently asked
SiO target or SiO evaporation pellets?
For thin optical films, evaporation is more common; for large-area sputtering a target is used. Both are available.
Why is the film index inconsistent?
SiO disproportionates into Si and SiO2 during heating, so the film composition depends on the source history.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.




Reviews
There are no reviews yet.