Silicon dioxide is the standard low-index layer in optical coatings and the standard insulator in thin-film electronics. It is also the material that most often exposes a process problem, because a slightly oxygen-deficient SiO2 film absorbs in the UV and shifts the coating design.
Specification
| Composition | SiO2 |
|---|---|
| Purity | 99.9–99.99% |
| Density | 2.65 g/cm³ |
| Melting point | 1710 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- Stoichiometry matters: SiOx with x below 2 absorbs in the UV.
- SiO2 targets are insulators — RF sputtering, with the target bonded for cooling.
- For thick layers, deposition rate is low; consider a rotatable for volume work.
End applications
- Low-index layers in optical filters
- Insulating layers in thin-film electronics
- Protective and passivation coatings
- Planarisation layers
Frequently asked
Can SiO2 be sputtered with DC?
No — it is an insulator. RF (or pulsed DC with a special arrangement) is required.
Why does my SiO2 film absorb?
Oxygen deficiency or contamination. Check the target stoichiometry and the base pressure.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.





Reviews
There are no reviews yet.