Niobium Pentoxide (Nb₂O₅) Sputtering Target

3N–4N (99.9–99.99%)DiscSintering

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Niobium pentoxide offers a higher index than Ta2O5 at lower cost, which makes it attractive for NIR filters and for high-index layers where laser damage is not the limiting requirement.

Specification

Composition Nb2O5
Purity 99.9–99.99%
Density 4.60 g/cm³
Melting point 1520 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • Higher index than Ta2O5 but slightly more absorbing in the UV.
  • Stoichiometry affects both index and absorption — specify for optical work.
  • Density above 97% is normal; lower density shows as scatter.

End applications

  • NIR and IR optical filters
  • High-index layers in AR stacks
  • Electrochromic films
  • Dielectric layers

Frequently asked

Is Nb2O5 a drop-in replacement for Ta2O5?

In many NIR designs yes, with a re-optimised stack. In the UV, absorption is higher.

What purity do you supply?

3N–4N depending on grade; the certificate states the level.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Niobium Pentoxide (Nb₂O₅) Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us