Bismuth oxide has an unusually high refractive index for a low-melting oxide, which makes it useful in optical coatings and in visible-light photocatalysis. Its low melting point (824 °C) means the target must be cooled and sputtered gently.
Specification
| Composition | Bi2O3 |
|---|---|
| Purity | 99.9% |
| Density | 8.90 g/cm³ |
| Melting point | 824 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- Low melting point — bond the target and keep power density down.
- High index makes it attractive for optical designs, but films can be oxygen-deficient.
- Bismuth is a heavy element; sputter yield is low compared with light oxides.
End applications
- Optical coatings and high-index layers
- Photocatalytic films
- Solid oxide and sensor research
- Decorative and iridescent coatings
Frequently asked
Why does my Bi2O3 film look metallic?
Oxygen deficiency. Bi2O3 reduces easily; increase the oxygen partial pressure or use a fully stoichiometric target.
Can Bi2O3 be sputtered without bonding?
Not reliably. At 824 °C the target softens quickly; a bonded, cooled assembly is required.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.