Tungsten wire at 3N5 purity, from 0.1 mm to 3.0 mm, straight or coiled. Tungsten has the highest melting point of any metal (3422 °C), which is why it is used for evaporation filaments, heater elements and high-temperature contacts.
Specification
| Metal | Tungsten (W) |
|---|---|
| Purity | 3N5 (99.95%) |
| Form | Wire |
| Dimensions | Ø 0.1–3.0 mm; straight or coiled; 100 mm–1 m lengths |
| Density | 19.25 g/cm³ |
| Melting point | 3422 °C |
| Packing | Vacuum-sealed, argon flushed; spool or flat pack in a foam-lined case |
| MOQ | By agreement — quoted per order |
| Lead time | 10–20 working days |
Tolerances and handling
- Tungsten wire is brittle at room temperature — avoid sharp bends and nicks, which become fracture points.
- For evaporation filaments, specify the coil geometry rather than just the diameter.
- At temperature tungsten reacts with oxygen; keep the vacuum below 10⁻⁴ mbar.
End applications
- Evaporation filaments and heaters
- Thermocouple wire and support pins
- Electron and ion source components
- High-temperature spring contacts
Frequently asked
What is the difference between doped and pure tungsten wire?
Potassium-doped tungsten (WAl) resists sag at temperature and is used for filaments; pure tungsten is used where contamination matters.
Can you supply 0.05 mm tungsten wire?
Yes, down to 0.05 mm on request; below that it is supplied as a special order.
Related reading: all wire, foil and solder products · high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.







Reviews
There are no reviews yet.