Platinum foil in 3N5 purity from 0.02 mm, for electrodes, crucible liners and evaporation sources. Platinum foil is used where a surface must stay inert at temperature — it does not oxidise, and it resists most molten salts and glasses.
Specification
| Metal | Platinum (Pt) |
|---|---|
| Purity | 3N5 (99.95%) |
| Form | Foil |
| Dimensions | Thickness 0.02–0.5 mm; width 10–100 mm; cut pieces to drawing |
| Density | 21.45 g/cm³ |
| Melting point | 1768 °C |
| Packing | Vacuum-sealed, argon flushed; spool or flat pack in a foam-lined case |
| MOQ | 100 g (samples from 10 g) |
| Lead time | 10–20 working days |
Tolerances and handling
- Platinum foil is soft and dents easily; handle with tweezers and store flat.
- For crucible liners, specify the exact dimensions — a loose liner behaves worse than a fitted one.
- Iron contamination from steel tools makes platinum brittle at temperature; use platinum or ceramic tools.
End applications
- Electrodes and crucible liners
- Evaporation source for thin films
- Catalyst samples and gauze
- Sealing and contact shims
Frequently asked
Why does platinum foil become brittle?
Contamination — iron, silicon or carbon from tools or the furnace. Once contaminated, the foil cannot be recovered by cleaning.
What is the thinnest foil you supply?
0.02 mm; thinner foil is available on request but is difficult to handle and pack.
Related reading: all wire, foil and solder products · high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.