Cuprous Oxide (Cu₂O) Sputtering Target

3N (99.9%)DiscSintering

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Cuprous oxide is a p-type semiconductor with a direct band gap near 2.1 eV, which makes it interesting for solar cells, photodetectors and transparent electronics. It is a different material from CuO, and the target phase decides which film you get.

Specification

Composition Cu2O (cuprous)
Purity 99.9%
Density 6.0 g/cm³
Melting point 1235 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • Cu2O and CuO are different targets — specify the phase.
  • Cu2O is metastable; deposition conditions can oxidise it further to CuO.
  • For solar work, the carrier mobility depends strongly on film quality.

End applications

  • p-type solar cell absorbers
  • Photodetectors
  • Transparent semiconductor research
  • Gas sensors

Frequently asked

How do I keep the film as Cu2O rather than CuO?

Control the oxygen partial pressure and the substrate temperature; too much oxygen gives CuO. Start from a phase-pure Cu2O target.

Is Cu2O available in production quantities?

Yes, but it is mainly a research and sensor material rather than a high-volume coating.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Cuprous Oxide (Cu₂O) Sputtering Target”

Your email address will not be published. Required fields are marked *