An optical coating is a stack of alternating high- and low-index layers, and the stack only performs as designed if each layer’s index and thickness are what the design assumed. That makes target purity, density and stoichiometry unusually important: a 1% deviation in index moves a filter’s centre wavelength.

Material selection by band

SiO2 Low index (n ≈ 1.46) · transparent 0.2–8 µm · RF · the standard low-index layer
TiO2 High index (n ≈ 2.3–2.6) · 0.35–7 µm · highest index of the common oxides; absorption rises if substoichiometric
Ta2O5 High index (n ≈ 2.1) · 0.3–8 µm · dense, low scatter, preferred for precision filters
Nb2O5 High index (n ≈ 2.2) · 0.35–8 µm · higher index than Ta2O5, good for NIR
Al2O3 Medium index (n ≈ 1.65) · 0.2–8 µm · hard, chemically stable, often a barrier layer
ZrO2 High index (n ≈ 2.1) · 0.25–10 µm · tough, good for laser coatings
HfO2 High index (n ≈ 2.0) · 0.22–10 µm · laser damage resistance, UV-capable

What decides the specification

  • Wavelength band — UV cuts the material list sharply; HfO2 and Al2O3 survive where TiO2 absorbs.
  • Laser damage threshold — density and included defects dominate; hot-pressed targets with fine grain and low porosity are preferred.
  • Layer count — a 50-layer filter needs targets sized for a full run, not a 100 g sample.
  • Deposition method — oxides are normally RF sputtered; some lines use reactive DC from metal targets, which shifts the control problem to the gas loop.

Target form and bonding

Oxide targets are brittle, so bonding and cooling matter as much as the material. We supply planar targets from 2 inch R&D sizes to 300 mm plates, indium or elastomer bonded to copper backing, with density and stoichiometry stated on the certificate. Rotary targets are available for high-volume lines.

What we supply

Frequently asked

Why does my TiO2 film come out absorbing?

Usually oxygen deficiency. Reactive sputtering with insufficient O2, or a target that has been reduced, produces substoichiometric TiOx, which absorbs in the visible. Check the target’s oxygen content and the gas loop.

Can one target be used for both e-beam and sputtering?

No. E-beam charges are granules or pellets in a liner; sputtering targets are dense discs or plates with a bonded backing. The material may be the same, the form is not.

Related reading: deposition methods compared · ceramic sputtering targets